Friday, September 18, 2009
Shutdown stsetch2 SNF 2009-09-18 02:16:37: Broken Wafer in Chamber
Observed very high helium leak rate (as previous users did) and wafer then broke in chamber. Wafer was a fusion bonded wafer but total thickness was near that of a standard wafer (600 um) and its use was cleared with a senior labmember.